Tuyouku water-based crystal varnish, with high gloss, high fullness, high hardness Long-lasting gloss, good reflectivity, excellent weather resistance, chemical resistance Excellent performance, suitable for various repair types in different environments.
Applicable base materia
Tuyouku surface of the primer of the series of products
Mixed ratio
use (Tuyouku) series of oil removal cleaners to remove wax, oil stains and other impurities.
25℃: The interval between layers is 10-15 minutes respectively. After spraying, it must be left for 15-20 minutes before heating and baking (temperature 45℃)
Repeated construction
Small particles and hanging places can be polished with wax after 2000# sandpaper after complete hardening.
Spraying tools and air pressure
geocentric spray gun (upper pot)
1.2- 1.5mm
3-5kg/c㎡
suction spray gun (lower pot)
1.4- 1.7mm
3-5kg/c㎡
Dry and solid time
mixing ratio/25℃
mixing ratio/25℃
mixing ratio/25℃
25min
mixing ratio/25℃
30min
mixing ratio/25℃
8h
Storage period
put it in a cool and dry place / 20℃, and the original cover can be stored for two years.
Packaging specifications
1L or 4L cans
Notes:
1. The primer film must be polished and cleaned before spraying (wet grinding 600#-800#, dry grinding 400#-600#) 2. If the base material has an old paint film that is not suitable, it is recommended to use the two-component water-based primer of the TuYouku series for sealing, and then spray the color paint, otherwise the bottom will bite and fall off. Phenomenons such as bubbles and floating colors. 3. Leave the 1k primer for 10-15 minutes after spraying, and spray the varnish as soon as possible. The long time will affect the adhesion. 4. Due to the high transparency of water-based paint, in terms of paint treatment, the color should be uniform, the flatness should be guaranteed, and there should be no sand marks, particles or unevenness, otherwise gold The paint layer will have problems such as silver poly, hair and a poor sense of metal. 5. The thickness of the spray film of the metal paint series is not easy to exceed 25um, otherwise it is prone to problems such as silver gathering and poor adhesion between layers. 6. After spraying a piece of metal plain paint, dry it in the air, and spray the next process after 10-15 minutes. 7. When the temperature is at the bottom of 5℃, it is recommended not to add water, but to add ethanol as water proportionally.