Tuyouku Water-based midway primer, is a multi-purpose quick-drying two-component primer,Products with excellent filling, good adhesion between layers, and good polishing, which can improve the fullness and gloss of the topcoat.
Suitable for substrate
metal surface, putty surface
Mixed proportion
D558 water-based midway primer
100%
primer curing agent
20%
Deionized water
20 – 30%
Available time after mixing
25℃:24h
Number of construction times
2-3Coating,30-50um
Interlayer interval time
the interval between layers is 10-15 minutes. After spraying, it must be left for 15-20 minutes before heating and baking, or self-drying.
Repeated construction
Small particles and hanging places can be polished with wax after 2000# sandpaper after complete hardening.
Spraying tools and air pressure
Geocentric spray gun (upper pot)
1.2-1.5mm
3-5kg/c㎡
Suction spray gun (lower pot)
1.7-1.8mm
3-5kg/c㎡
Dry and solid time
Temperature
DG580 curing agent 25℃
non-stick dust time
15 min
ouchable time
25 min
assembly time
6 h
Storage period
put it in a cool and dry place / 20℃, and the original cover can be stored for two years.
Packaging specifications
1L or 4L cans
Notes:
1. When the temperature is below 10℃ , it is recommended to bake in a baking room of 40-50℃ for 30 minutes to facilitate the solidification of the paint film. 2. The curing agent must be used correctly, otherwise the paint film may not dry completely. 3. When the temperature is at the bottom of 5℃, it is recommended not to add water, but to add ethanol as water in proportion.
SR777 water-based oil inhibitor
Product features:
Tuyouku water-based special oil inhibitor is a top paint additive, which is used to eliminate paint film problems such as fish eyes or shrinkage in the paint film.
Supporting products
multi-functional plain paint, pearl silver powder paint and varnish
Add proportion
SR777 products with 0.5-2 can lids (about 4-15g) is SR777
Storage period
put it in a cool and dry place / 20℃, and the original cover can be stored for two years.
Packaging specifications
1L
Notes:
1. The amount added should not be too much, otherwise the paint film is prone to dark bubbles or pinholes. 2. If the beading situation is serious, it must be polished and flattened after the paint film is dry, and sprayed again after adding anti-bead water.